耐腐合金材料选用中英文对照表:
序号 | 牌号 | 代号 | 适用介质 |
1 | F30%CrMo | Cr30 | 是含固量达35%腐蚀性介质的理想选材,如磷酸萃取料将等类似腐蚀磨蚀性介质,目前居国内领先水平。 |
2 | 1Cr18Ni9Ti | 18-8 | 碱液、醋酸、稀硝酸。 |
3 | 00Cr20Ni25Mo4 | UB6 | 含一定数量的Cl-F- SO24-磷酸、硫酸及高温醋酸抗点蚀和晶间腐蚀。 |
4 | 00Cr14NiSi4 | C4 | 全浓度硝酸、特别适用浓硝酸、事目前浓硝酸用钢综合性最好的铸材。 |
5 | 0Cr12Ni25Mo3Cu3Si2Nb | 941 | 全浓度常温硫酸、特别适用100℃以下的中等浓度(50%)硫酸。 |
6 | 00Cr10Ni20Mo1.5Si6Cu | SS920 | 高温浓硫酸,t≤130℃,浓度93-98% |
7 | 0Cr21Ni32Mo2Cu3 | 20#合金 | 高温浓硫酸,t≤130℃,浓度为40%左右。 |
8 | Z180C13 | DF2 | 含固量达70%磨蚀性介质。 |
9 | 0Cr26Ni5Mo2Cu3 | CD-4MCu | 含固稀硫酸,磷酸,耐磨,耐蚀。 |
10 | 0Cr24Ni20Mo2Cu3 | K合金 | ≤60℃各种浓度的硫酸。 |
11 | 00Cr25Ni6Mo2 | MM-4 | 硝酸磷肥专用钢。 |
12 | 0Cr18Ni9 | 304 | 稀硝酸,有机酸。 |
13 | 00Cr18Ni9 | 304L | 稀硝酸,有机酸,抗晶间腐蚀。 |
14 | 0Cr18Ni12Mo2Ti | Mo2Ti | 稀硝酸,磷酸,有机酸。 |
15 | 0Cr18Ni12Mo2 | 316 | 稀硝酸,磷酸,有机酸。 |
16 | 00Cr18Ni12Mo2 | 316L | 稀硝酸,磷酸,有机酸,抗晶间腐蚀。 |
17 | 0Cr20Ni25Mo5Cu | 904 | 70℃以下各种浓度硫酸,抗晶间腐蚀。 |
18 | 0Cr30Ni42Mo3Cu2 | 804 | 烧碱蒸发及904仍不抗蚀等。904仍不抗蚀介质。 |
19 | 0Cr20Ni42Mo3Cu2 | 824 | 904仍不抗蚀介质 |
20 | 0Cr18Ni5Mo5 | NH55 | 海水。 |
21 | 0Cr20Ni33Mo3Cu3Nb | 20Cb3 | 各种浓度的硫酸腐蚀。 |
22 | 0Cr24Ni33Mo2.5Cu3Ti | 3#4# | 含20%固相的稀硫酸磨损腐蚀。 |
23 | 0Cr16Ni4Cu3Nb | CB-7Cu | 砂浆磨蚀,钾肥生产时卤水的磨、腐蚀。 |
24 | 00Cr30Ni40Mo4Cu3 | Lewmet55 | 125℃高温发烟硫酸腐蚀。 |
25 | 00Ni65Cu28 | Monel | 氢氟酸、硅氟酸、高温烧碱。 |
26 | 00Ni65Mo28 | 哈氏B | 全浓度盐酸。 |
27 | 塑料FEP | F46 | 各种酸、碱、盐、氧化剂等介质。 |
28 | UHMWPE | 80℃以下含悬浮固体颗粒的酸、碱、盐介质、耐磨损。 | |
29 | Fluoride alloy | 180℃以下强腐蚀介质。 |
No. | Material rating number | Code | Suitable media |
1 | F30%CrMo | Cr30 | Leading the pack in the domestic market, it is an ideal material for corrosive media containing up to 35% of solid., such as phosphoric acid extract slurry or similar corrosive medium. |
2 | 1Cr18Ni9Ti | 18-8 | Alkali liquid, acetic acid, diluted nitric acid |
3 | 00Cr20Ni25Mo4 | UB6 | Phosphoric acid, sulfuric acid, and high temperature acetic acid containing certain amount of CL-,F-SO24-. Resistant to pitting and inter granular corrosion. |
4 | 00Cr14NiSi4 | C4 | Full concentration nitric acid, especially concentrated nitric acid. It is the best cast steel in comprehensive performance for concentrated nitric acid available at present. |
5 | 0Cr12Ni25Mo3Cu3Si2Nb | 941 | Full concentration constant temperature sulfuric acid especially middle concentrated (ca.50%) sulfuric acid below 100℃ |
6 | 00Cr10Ni20Mo1.5Si6Cu | SS920 | High temperature sulfuric acid, t≤130℃,concentration 93-98% |
7 | 0Cr21Ni32Mo2Cu3 | 20#合金 | High temperature sulfuric acid, t≤130℃, concentration ca.40% |
8 | Z180C13 | DF2 | Corrosive medium containing up to 70% of solid. |
9 | 0Cr26Ni5Mo2Cu3 | CD-4MCu | Suitable for diluted sulfuric acid and phosphoric acid containing solid. It is anti-abrasive and anti-corrosive. |
10 | 0Cr24Ni20Mo2Cu3 | K合金 | Sulfuric acid of various concentrations at≤60℃ |
11 | 00Cr25Ni6Mo2 | MM-4 | Special steel for nitric acid and phosphoric fertilizer. |
12 | 0Cr18Ni9 | 304 | Diluted nitric acid and organic acids. |
13 | 00Cr18Ni9 | 304L | Diluted nitric acid and organic acids. Resistant to inter granular corrosion. |
14 | 0Cr18Ni12Mo2Ti | Mo2Ti | Diluted nitric acid, phosphoric acid, and organic acids. |
15 | 0Cr18Ni12Mo2 | 316 | Diluted nitric acid, phosphoric acid, and organic acids. |
16 | 00Cr18Ni12Mo2 | 316L | Diluted nitric acid, phosphoric acid, and organic acids. Resistant to inter granular corrosion. |
17 | 0Cr20Ni25Mo5Cu2 | 904 | Sulfuric acid of various concentrations at ≤70℃.Resistant to inter granular corrosion. |
18 | 0Cr30Ni42Mo3Cu2 | 804 | Evaporation of caustic soda, and those media whose corrosiveness is beyond the capability of 904. |
19 | 0Cr20Ni42Mo3Cu2 | 824 | Those media whose corrosiveness is beyond the capability of 904. |
20 | 0Cr18Ni5Mo5 | NH55 | Sea water |
21 | 0Cr20Ni33Mo3Cu3Nb | 20Cb3 | Corrosion of sulfuric acid of various concentrations. |
22 | 0Cr24Ni33Mo2.5Cu3Ti | 3#4# | Abrasion and corrosion of diluted sulfuric acid containing 20% solid phase. |
23 | 0Cr16Ni4Cu3Nb | CB-7Cu | Corrosion of sand slurry, abrasion and corrosion of halogen liquid in the production of potassium fertilizer. |
24 | 00Cr30Ni40Mo4Cu3 | Lewmet55 | Corrosion of 125℃ high temperature fuming sulfuric acid. |
25 | 00Ni65Cu28 | Monel | Hydrofluoric acid, silicofluoric acid, high temperature caustic soda. |
26 | 00Ni65Mo28 | 哈氏B | Full concentration hydrochloric acid. |
27 | 塑料FEP | F46 | Various acids, alkalis, salts, oxidants, etc. |
28 | UHMWPE | Acids, alkalis, and salts containing suspended solid granules below 80℃. | |
29 | Fluoride alloy | Strong corrosive media below 180℃. |